Gold recovery in waste electrolyte

    The waste electrolyte contains 250 to 300 g/l of gold . Commonly used recovery methods are replacement method and reduction method.
    Replacement: replacing zinc powder, the reaction is:

    2HAuCl 4 +3Zn=2Au↓+3ZnCl 2 +2HCl

    Before using zinc powder to replace the waste electrolyte, it should be boiled and the nitrate should be washed to avoid gold returning. At the time of replacement, the pH is 1 to 2, so as to avoid the solution of zinc salt water to 30 g, which prevents the precipitation of gold.
    Reduction: ethylene sulfite can be used iron sulfate or reduction reactions are of formula:

    3FeSO 4 +HAuCl 4 = Au↓+FeCl 3 +Fe 2 (SO 4 ) 3 + HCl

    Na 2 SO 3 +2HCl=2NaCl+H 2 O+SO 2 ↑

    2HAuCl 4 +3SO 2 +6H 2 O=2Au↓+8HCl+3H 2 SO 4

    In addition to precious metals, ferrous sulfate has almost no reduction effect on other metals, so it is beneficial to improve the purity of the reduced gold. However, the reduction reaction of ferrous sulfate is slow, the reaction is not thorough, and the tail liquid needs to be further treated with zinc powder.
    If the waste electrolyte contains nitric acid, it should be heated and boiled before reduction to remove free nitric acid. Large particle sponge gold can be obtained by appropriate heating during reduction. In order to enhance the reduction of sponge gold, it has been proposed to add 0.3 g/L of polyethylene glycol as a coagulant to the solution.

    Glass Edge Finishing Machine

    Glass Edge finish machine LJMB95 is used to carry out rough grinding and chamfering after the cutting of the original glass sheet. With easy and simple operation, low labor intensity and high production efficiency, it is indispensable for safety production of all kinds of windows and doors. It is suitable for the edge-finishing of the raw glass for insulating glass.

    Glass Edge Finishing Machine,Custom Glass Edging Machine,Manual Belt Grinding Machine,Glass Sides Grinding Machine

    JINAN KATION TRADING CO.,LTD , https://www.machinerychinese.com

    Previous Post: Method for purifying mercury-containing exhaust gas
    Next Post: Titanium dioxide production process technology - post-treatment
    Home
    Recent Posts
    • Inhibition and inhibitor of gangue minerals in m…
    • What is electromagnetism?
    • Study on Acid Leaching of Low Grade Primary Copp…
    • Structure and composition of heap immersion mat
    • Tailings facility
    • Automatic adjustment rod mill feeding set value …
    • Method for purifying mercury-containing exhaust …
    • Gold recovery in waste electrolyte
    • Titanium dioxide production process technology -…
    • Several application fields and actual cases of i…
    • Latest developments in iron ore beneficiation
    • Multi-angle adjustment to increase the productiv…
    • Pull rivet nut professional knowledge introducti…
    • Simultaneous treatment of nickel-based waste raw…
    • Several representations of the productivity of t…
    • Dongfeng Volvo JV will be listed in the second h…
    • GB6722-1986 blasting safety regulations (10)
    • Double curved wave bed shaker
    • 钽铌Secondary resource recovery
    • Cyanide-containing wastewater recycling example